1 / 3
| Item | Unit | Typical Values |
|---|---|---|
| Width | mm | 30–1200 |
| Thickness | micron | 12–100 |
| Shrinkage | % | TD: 5–60 | MD: 1–40 |
| Shrink Temperature | ℃ | 90–150 |
| Proportion | g/cm³ | 1.4 |
| Tensile Strength | MPA | TD: ≥42 | MD: ≥50 |
| Transverse Elongation at Break | % | TD: ≥70 | MD: ≥50 |
| Tear Strength | KN/M | TD: ≥60 | MD: ≥45 |